Thermanit GE-316L德國蒂森不銹鋼焊絲
Thermanit GE-316L TIG rod
Classifications high-alloyed
EN ISO 14343-A: AWS A5.9:
W 19 12 3 L ER316L
Characteristics and field of use
Stainless resistant to intercrystalline corrosion and wet corrosion up to 400 °C (752 °F). Corrosion-
resistance similar to matching low-carbon and stabilized austenitic 18/8 CrNiMo steels/cast
steel grades. For joining and surfacing application with matching and similar – non-stabilized and
stabilized – austenitic CrNi(N) and CrNiMo(N) steels and cast steel grades.
Marks (rods0nly)
W 19 12 3L / ER316L
Base materials
TüV-certified parent metal
1.4583 – X10CrNiMoNb18-12 S31653, AISI 316L, 316Ti, 316Cb
Typical composition of welding rod (Wt-%)
C Si Mn Cr Ni Mo
0.02 0.5 1.7 18.5 12.3 2.6
Mechanical properties of all-weld metal
Heat Treatment Yield strength
0.2%
Tensile
strength
Elongation
(L0=5d0)
Impact values
in J CVN
MPa MPa % +20°C:
untreated 450 580 35 100
Operating data
Polarity = – Shielding gas (EN ISO 14175):
I1
Dimensions (mm)
1.0 1.2 1.6 2.0 2.4 3.2 4.0